1
|
2
|
3
|
4
|
|
Correct Number/Placement
of Arc Weld Beads
|
Missing 1 stringer
and weave bead, more than 1 stringer/weave fully above
lower 2" of plate
|
Most required beads
present, 1 partially above the lower 2" of the plate,
missing only 1 weave
|
All required beads
present, somewhat above the lower 2" of the plate
|
All 4 stringers and
all 3 weaves are within the lower 2" of the plate.
|
____
|
Clean/Slag Free
Plate Surface
|
Approximately 2/3 of
the slag has been removed, heavy hammer marks
|
Approximately 3/4 of
the slag has been removed, moderate hammer marks
|
Approximately 90% of
slag has been removed, small to no hammer marks
|
100% of slag removed,
No hammer marks
|
____
|
Straightness of
beads/spacing
|
Excessive spacing/bunching,
extremely crooked lines
|
Moderate spacing/bunching,
crooked lines
|
Near Correct spacing,
stringer beads have small change from parallel to plate
edge
|
1/2" spacing between
stringer beads parallel to plate edge
|
____
|
Student observes
all safety practices during the project
|
Moderately uniform
beads with some small variation in both width and thickness
|
Minor breaks from uniformity
of width and thickness, very small variations
|
Beads are nearly uniform
in width and thickness, no more than 1 high/low spot
or thick/thin spot
|
Beads are uniform in
width and thickness
|
____
|
Correct shop safety/setup/cleanup
is demonstrated by the student.
|
2-3 minor reminders
on setup or cleanup procedures, 2-3 minor reminders
on safe shop practices
|
1 minor reminder on
setup or cleanup procedures, 1 minor reminder on safety
practices
|
All assigned setup
and cleanup procedures are demonstrated, No safety violations
|
All setup and cleanup
procedures demonstrated, student helps others with setup/cleanup
correctly, No safety violations
|
____
|
|
|
|
|
Total---->
|
____
|